Gunlake Early Strength S40 22@4 40 MPa Ready-Mix Concrete - New South Wales, AU

Concrete In-situ 40MPa
Australia
Supplier
GCPL
Gunlake Concrete Pty Ltd
Description
The product is a 40 MPa early strength ready-mix concrete with a density of 2360 kg/m3. It is designed for applications such as pre and post tensioning and uses 20/10mm aggregates.
Specifications
Density2360 kg/m3Mix codeS40 22@4Mix description40MPa (22MPa@4days), 20/10mm aggConcrete applicationpre_and_post_tensionCoarse aggregate size20 mmCompressive strength mpa40 MPa
kg CO2-eq./m3
Info
A1-A3A1-A2-A3-A4-A5-B1-B2-B3-B4-B5-B6-B7-C1C2C3C4D
EPD
Certifications
ISO 14025
EN 15804+A2